Tungsten Carbide Cobalt Powder – LA-3203-27 (-325 +5u) WC-Co 83/17, sintered and crushed

Out of stock
- Material Specificaiton
- Product Application
- Useful Documents
- Equivalents
- Method
- REVIEW
Material Specificaiton for LA-3203-27 (-325 +5u) WC-Co 83/17, sintered and crushed
Chemical Compositon Requirements (By weight percent)
Element | Minimum | Maximum | Target |
Aluminum | - | - | - |
Boron | - | - | - |
Carbon | 4.50% | 5.60% | 5.05% |
Chromium | - | 0.50% | 0.25% |
Cobalt | 15.00% | 18.00% | 16.50% |
Free Carbon | - | - | - |
Iron | - | 1.50% | 0.75% |
Manganese | - | - | - |
Molybdenum | - | - | - |
Nickel | - | 0.50% | 0.25% |
Oxygen | - | - | - |
Silicon | - | - | - |
Sulfur | - | - | - |
Tungsten | 76.00% | - | 76.00% |
Vanadium | - | - | - |
Rotap Sizing Requirements (Weight Percent Per ASTM B214)
U.S. Mesh Passing Sieve X Retained | - | - | Min. | Max. |
- | - | 140 Mesh | - | - |
140 Mesh | X | 170 Mesh | - | - |
170 Mesh | X | 200 Mesh | - | - |
200 Mesh | X | 230 Mesh | - | - |
230 Mesh | X | 270 Mesh | - | 0.00% |
270 Mesh | X | 325 Mesh | - | 0.50% |
325 Mesh | X | D | 99.50% | - |
Sub-Sieve Sizing Requirements (Volume Percent Per ASTM B822)
Micron Channel | Min | Max |
-22 μ | 70.00% | - |
-5.5 μ | - | 8.00% |
- | - | - |
- | - | - |
- | - | - |
- | - | - |
- | - | - |
Physical Properties Requirements
Testing Procedure | Minimum | Maximum |
Hall Flow (per ASTM B213) | - | - |
Apparent Density (per ASTM B212) | - | - |
Mean Value (per ASTM B222) | - | - |
D10 (per ASTM B222) | - | - |
D50 (per ASTM B222) | - | - |
D90 (per ASTM B222) | - | - |
These products are ideal for:
- Landing Gears
- Mid-span shrouds
- Pump seals
- Aircraft Flap Tracks
- Exhaust fans
- Crushing Rollers
Equivalents:
- Amperit 525.1
- Diamalloy 2005
Method:
- Air Plasma Spray
- HVOF
Request a Quote
Fill the form below and we’ll answer as soon as possible